Hc FeCr Lump
video

Hc FeCr Lump

The traditional return oxygen blowing method is used to smelt ultra-low carbon stainless steel, with a chromium content of 8% to 9%. However, during reduction refining, microcarbon ferrochrome or metallic chromium accounting for more than 10% of the molten steel needs to be added, and the alloy cost accounts for more than 10% of the molten steel. The main part of the cost of low carbon stainless steel liquid steel.
Send Inquiry
Product Introduction
Smelting Ultra-Low Carbon Stainless Steel By High Carbon Ferrochromium Back Blowing Method

 

In recent years, with the extensive application of stainless steel in society, stainless steel scrap resources have become increasingly abundant. At the same time, a large amount of stainless steel castings are returned to the stainless steel castings in the steel casting plant. In order to reduce production costs, on the basis of the return method to smelt ultra-low carbon stainless steel, the high-carbon ferrochrome return oxygen blowing method is used to smelt ultra-low carbon stainless steel to improve The chromium content of the furnace charge can use less or no expensive micro-carbon ferrochrome or metallic chromium, which has considerable economic benefits.

 

nitrided ferro chrome

Industrial Ferrochrome

 

The high carbon ferrochromium return oxygen blowing method is a smelting method that uses returned materials to recover alloy elements and remove gases and inclusions through oxygen blowing and decarburization to ensure the performance requirements of the steel. When batching, increase the amount of chromium in the charge. In addition to a large amount of returned materials, an appropriate amount of high-carbon ferrochromium can be added to make the chromium content in the charge reach a higher level, higher than the specification standard.

 

medium carbon ferro chrome

Low Carbon Ferro Chrome

 

Stainless steel is smelted by the return oxygen blowing method of high carbon ferrochrome. The burning loss of chromium has been fully considered during the batching process, and the chromium content has been adjusted to a higher content. During the oxygen blowing decarburization process, the thermodynamic conditions of carbon and chromium balance have been fully utilized. Remove carbon and preserve chromium to minimize the oxidation of chromium. When the carbon is reduced to the requirement, the chromium content is close to or reaches the specification standard. Without adding or adding a small amount of micro-carbon ferrochromium, the chromium content can reach the specification standard after reduction.

 

Low Carbon Ferro Chrome

 

Grade Chemical Composition(%)
Cr C Si P S


Micro carbon
FeCr-1 58-68 0.03-0.15 1.0-2.0 0.03-0.06 0.025-0.03
FeCr-2 63-68 0.03-0.15 1.0-2.0 0.03-0.06 0.025-0.03


Low carbon
FeCr-3 58-68 0.25-0.5 1.5-3.0 0.03-0.06 0.025-0.03
FeCr-4 63-68 0.25-0.5 1.5-3.0 0.03-0.06 0.025-0.03


Medium carbon
FeCr-5 58-68 1.0-4.0 1.5-3.0 0.03-0.06 0.025-0.03
FeCr-6 63-68 1.0-4.0 1.5-3.0 0.03-0.06 0.025-0.03


High carbon
FeCr-7 58-68 4.0-10.0 3.0-5.0 0.03-0.06 0.03-0.06
FeCr-8 63-68 4.0-10.0 3.0-5.0 0.03-0.06 0.03-0.06

 

High Carbon Ferro Chrome

carbon ferro chrome

High Carbon Ferro Chrome Low Silicon

 

 

 

ferro chrome alloy

Charge Chrome

 

How To Contact ZhenAn


       

        info@zaferroalloy.com

       25th Floor, Huafu Commercial Center, Wenfeng District, Anyang City, Henan Province, China

       Phone: +8615896822096

       Whatsapp: +8615896822096

 

Hot Tags: hc fecr lump, China hc fecr lump manufacturers, suppliers, factory, low carbon ferro chrome lump price, high Carbon Ferro Chrome, medium carbon ferrochrome lump, Nitrited Low Carbon Ferro Chrome lump, High Carbon Ferro Chrome Low Silicon lump, nitrided ferro chrome lump

Send Inquiry

Home

Phone

E-mail

Inquiry