Fire prevention should be strictly enforced during batching. Due to the flammable and explosive nature of the charge, strict fire prevention measures are required. The mixing process must have strict closed smoke exhaust and dust removal facilities.

High purity femo manufacture
The normal signs of the smelting process are:
(1) The reaction is intense, the exhaust smoke is thick, the reaction is uninterrupted, there is no splashing, the reaction ends clearly, and there is no prolongation. After the reaction, the smoke is bright and clear.
(2) When discharging slag, the slag has good fluidity and a slight sticking phenomenon. After cooling, the surface of the slag in the slag tank is convex and shiny, and the slag sample is dark green.

Ferro Molybdenum Metal manufacture
(3) When pulling out the furnace barrel, there is a phenomenon of slag wire pulling, and the upper slag cover of the ferromolybdenum ingot is slightly concave.
(4) The reaction time is within the range of 2-10 minutes.