Ferrosilicon Manganese 65
Application of high carbon ferromanganese: High carbon ferromanganese can be divided into electric furnace high carbon ferromanganese and blast furnace high carbon ferromanganese according to different processing techniques. Among them, high-carbon ferromanganese in electric furnaces is mainly used as deoxidizer, desulfurizer and alloy additive in the steelmaking process. In addition, with the advancement of medium and low carbon ferromanganese production technology, high carbon ferromanganese can also be used to produce medium and low carbon ferromanganese. In addition, blast furnace high carbon ferromanganese can be used as deoxidizer or alloying element additive in steelmaking.

Ferromanganese 65 Alloy
High carbon ferromanganese production process:
blast furnace method
High-carbon ferromanganese was first produced in a blast furnace with high output and low cost. It is still widely used at home and abroad.
The blast furnace method is to add manganese ore, coke, lime and other materials into the blast furnace for smelting to obtain blast furnace ferromanganese containing 52%~76% manganese/0.4%~0.6 phosphorus. Since the only difference between the blast furnace and the electric furnace for smelting high-carbon ferromanganese is the different heat sources, the furnace structure, geometry and operation methods of the two furnaces are different, but the principles of smelting high-carbon ferromanganese in the two furnaces are the same.
However, the two furnaces use the same manganese ore for smelting, so the phosphorus content of the products obtained is different. The blast furnace product is 0.07%~0.11% higher than the electric furnace product. This is because the amount of coke in the charge composition of blast furnace smelting is 5 to 6 times that of electric furnace smelting, so more phosphorus in the coke is transferred into the alloy, and the furnace temperature during blast furnace smelting is lower, so during the smelting process The volatilization of phosphorus is about 10% lower than that of electric furnaces.

Ferrosilicon Manganese 65
Electric furnace method
There are three methods for smelting high carbon ferromanganese using the electric furnace method.
1) Fluxless method. For manganese-rich ores with high manganese oxide content, ferromanganese can be smelted using a flux-free method. Lime is not added to the charge during smelting. The equipment and operation are similar to ferrosilicon, and acidic slag is used under the condition of insufficient reducing agent. The furnace temperature It is about 1320~1400℃ lower than the flux method. Using this method to produce not only qualified high carbon ferromanganese, but also low phosphorus, low iron and manganese-rich slag containing more than 35% manganese for smelting manganese alloys. At this time, the distribution of manganese is as follows: the alloying rate is 58% to 60%, the slag rate is 30% to 32%, and the volatilization rate is 10%. Obviously, the flux-free method for smelting high-carbon ferromanganese must use manganese-rich ore with high manganese content, and requires a relatively low phosphorus content in the ore. Although the manganese recovery rate of this method is low, most of the manganese can be recovered when smelting manganese alloys with manganese-rich slag, and the total manganese recovery rate is higher than that of flux. The process of smelting high carbon ferromanganese by the solvent-free method is continuous. The charge is continuously added into the furnace along with the melting process. The batch can be composed of 300kg manganese ore, 60~70kg coke, and 15~20kg steel scraps. During solvent-free smelting, the unit power consumption of the product is very low, and it is easy to produce low-silicon high-carbon ferromanganese because most of the silicon is enriched in the slag.
2) Solvent method. The solvent method is a commonly used method for smelting high carbon ferromanganese. In addition to manganese ore and coke, the charge composition also includes lime and high alkalinity slag during smelting. The alkalinity is B=1.3~1.4. Sufficient reducing agent is used to reduce the manganese content in the waste slag as much as possible and improve the recovery rate of manganese. This method is used to smelt high-carbon ferromanganese with poor and rich manganese ores. This method will be discussed in detail later.
3) Less solvent method. This method uses the so-called "weakly acidic slag method" between the solvent method and the solvent-free method. This method is to add an appropriate amount of lime or limestone to the furnace charge to control the ratio of the slag basicity m (CaO)/m (SiO2) or m (CaO+MgO)/m (SiO20) between 0.6 and 0.8. It can not only improve the recovery rate of manganese, but also obtain slag containing 25% to 30% manganese and an appropriate amount of CaO. This slag can be added into the furnace charge for smelting silicon-manganese alloy, which can save lime and reduce the risk of lime deliquescence. Increase the amount of dust in the charge, thereby improving the air permeability of the charge. Foreign electric furnace smelting of high-carbon ferromanganese mostly uses acidic methods such as solvent-free method and flux-less method. In the 1950s, our country also adopted a flux-free method for smelting, using manganese-rich ore containing 46% to 47% manganese to produce carbon ferromanganese containing 76% manganese and 80% manganese, and at the same time obtaining manganese-rich slag containing 35% to 40% manganese. . However, because there are many poor manganese ores in my country, the solvent method or a small amount of solvent method is currently used.