Mechanical Properties of Zirconium Foil

Standards and Grades

Zirconium foil and strip are covered by ASTM B551, which defines the requirements for zirconium and zirconium alloy sheet, strip and plate. The common grades are R60702, known as Zr702, which is commercially pure zirconium, and R60705, known as Zr705, which is a zirconium-niobium alloy containing about 2.5 percent niobium. High-purity zirconium grades with very low hafnium content are also available for nuclear service.

Tensile Strength Levels

The tensile strength of zirconium foil depends on grade and temper. Annealed pure zirconium foil shows a tensile strength around 300 MPa, while zirconium-niobium grades such as Zr-2.5Nb and Zr-1.0Nb reach about 600 MPa in the worked or heat-treated condition. ASTM B551 specifies minimum tensile strengths of about 380 MPa for annealed R60702 and about 550 MPa for annealed R60705 material.

Yield Strength and Elongation

Yield strength follows the same ranking as tensile strength: annealed pure zirconium yields at about 200 to 250 MPa, while zirconium-niobium grades yield at roughly 380 MPa and above. Elongation in the annealed condition is generous, typically above 16 percent, which allows foil to be formed, stamped and welded without cracking. The combination of moderate strength and high ductility is the reason zirconium foil is preferred for chemical equipment linings and seals.

Hardness and Forming Behaviour

Zirconium has a hardness of about 180 to 200 Vickers in the annealed condition, rising with cold work and alloying. The material has a hexagonal close-packed crystal structure, which gives it anisotropic behaviour and a tendency to spring back during forming. Tooling and process design must therefore account for the elastic recovery of zirconium foil, especially in deep drawing and bending operations.

Factors Affecting Mechanical Properties

Cold rolling increases strength while reducing ductility, and subsequent annealing restores formability, so foil is often supplied in the annealed condition. Interstitial impurities, especially oxygen, nitrogen and hydrogen, have a strong hardening and embrittling effect on zirconium. Controlled processing and clean surfaces are essential to keep interstitial contents within specification and preserve reliable mechanical performance.

Practical Selection Guidance

For corrosion service in chemical plants, annealed Zr702 foil offers the best combination of corrosion resistance, ductility and weldability. For higher strength requirements, Zr705 or other zirconium-niobium grades are preferred. Buyers should specify grade, temper, thickness tolerance and the applicable standard to ensure that the delivered foil matches the mechanical property requirements of the application.

Frequently Asked Questions

Q: Which standard covers zirconium foil?
ASTM B551 covers zirconium and zirconium alloy strip, sheet and plate, including foil thicknesses.

Q: What is the tensile strength of annealed pure zirconium foil?
Annealed pure zirconium foil shows a tensile strength of about 300 MPa, with ASTM B551 requiring about 380 MPa minimum for R60702.

Q: What is the difference between Zr702 and Zr705?
Zr702 is commercially pure zirconium while Zr705 contains about 2.5 percent niobium for higher strength.

Q: Why is zirconium foil ductile enough for forming?
In the annealed condition zirconium foil has elongation typically above 16 percent, which supports stamping, bending and welding.

Q: Which impurities embrittle zirconium?
Oxygen, nitrogen and hydrogen are the main interstitial impurities that harden and embrittle zirconium.

Q: How does cold work change the mechanical properties of zirconium foil?
Cold rolling increases strength and hardness while reducing ductility, and a subsequent anneal restores formability, so the temper and heat treatment must be specified together with the grade.