Product Structure
From a materials point of view a magnesium ingot is composed of a magnesium matrix and a population of second-phase particles formed by alloying and impurity elements. The matrix provides the characteristic low density of about 1.74 g/cm3, good machinability and high specific strength. The second phases and solute elements modify strength, creep behaviour, corrosion resistance and castability. Understanding this two-part structure is the key to selecting the right ingot for a given process.
The magnesium matrix determines the base properties of the ingot:
Commercial magnesium ingots are graded by magnesium content, with common designations such as Mg9995 and Mg9990 referring to minimum magnesium contents of 99.95 and 99.90 percent respectively under standards such as GB/T 3499. The matrix determines the base properties:
Density of approximately 1.74 g/cm3, the lowest of the common structural metals.
Melting point of 650 deg C and a boiling point of about 1090 deg C.
Good machinability, since magnesium cuts cleanly at high speed with low cutting forces.
Ready reactivity with oxygen, which is why molten magnesium requires protective cover gas and magnesium products require careful storage.
Alloying Elements and Impurities
The structure of the ingot is defined as much by the elements present in small quantities as by the magnesium itself.
Aluminium and zinc: the basis of the common Mg-Al-Zn casting alloys, contributing strength and castability.
Manganese: added to improve corrosion resistance by controlling the effect of iron.
Silicon: present in some alloys and in feedstock for aluminium alloying.
Iron, nickel and copper: the three most damaging impurities, because they sharply increase corrosion rate even at very low levels. Specifications set tight maxima for each.
Chloride: residual flux salts from electrolytic production raise corrosion risk and are limited in the specification.
The practical consequence is that a high nominal magnesium content is not sufficient. A grade with 99.9 percent magnesium but excessive nickel or chloride will corrode far faster than a better-balanced ingot of the same nominal purity.
Grain Structure and Cast Quality
Magnesium ingots are produced by casting molten metal into moulds, and the casting conditions determine the grain structure, the amount of shrinkage porosity and the distribution of second phases. A sound ingot has a fine, uniform grain structure with no significant internal voids, no slag or flux inclusions and no segregation bands. Poor cast structure shows up downstream as inconsistent melting behaviour, variable recovery during alloying and surface defects in castings. Where the ingot is to be remelted for critical castings, the supplier's casting practice deserves as much attention as the chemical analysis.
Surface Quality
Magnesium oxidises readily, so the ingot surface carries a thin grey oxide film, sometimes with a white or dark appearance where the oxide is thicker. Acceptable limits on oxidation and contamination should be agreed, because heavy oxidation, corrosion staining and adherent flux residue all indicate poor protection during casting or storage. The surface should be free from cracks, folds, blowholes and cold shuts, since these trap moisture and salts. Magnesium ingots are commonly coated or wrapped for protection, and the coating should be removable without contaminating the melt.
Dimensional Accuracy and Weight Control
Ingot dimensions and weight are specified for a practical reason: a melting shop charges by weight, and consistent ingot weight simplifies batching and furnace control. Typical specifications state a nominal weight with a tolerance, together with limits on length, width and thickness. Oversize or irregular ingots do not stack or feed correctly, while undersized material creates handling losses. Consistent dimensions also indicate disciplined casting practice.
Selection Tips
Define the process first. Aluminium alloying, pressure die casting and steel desulfurisation each impose different impurity limits.
Check iron, nickel and copper limits specifically, not just the magnesium content.
Confirm chloride content if the ingot will be used in wet or corrosive service.
Ask for the cast lot analysis rather than a typical analysis, and keep heat traceability.
Verify surface condition and packaging, especially for shipment through humid regions.
Confirm ingot weight and dimensions against your charging equipment before ordering.
Correct storage and handling protect both the material and the workplace:
Magnesium must be kept dry, because damp material reacts and generates hydrogen. It should be stored away from acids, chlorides and oxidising agents, in a covered, well-ventilated area, separated from other combustible materials. Magnesium is a fire risk in finely divided form; solid ingots are easier to manage but still require appropriate protection against heat sources. Spilled magnesium powder or machining fines must never be allowed to accumulate.
Frequently Asked Questions
Q: What does the grade designation Mg9995 mean?
It indicates magnesium with a minimum content of 99.95 percent. Other designations such as Mg9990 indicate a minimum of 99.90 percent. Impurity limits are specified separately for each grade.
Q: Which impurities matter most in magnesium ingots?
Iron, nickel and copper have the greatest effect on corrosion resistance and are strictly limited, along with chloride from electrolytic production.
Q: Why is ingot weight consistency important?
Melting shops charge by weight, so consistent ingot weight and dimensions simplify batching, improve furnace control and reduce handling losses.
Q: Can oxidised magnesium ingots still be used?
A light protective oxide film is normal, but heavy oxidation, corrosion staining and flux residue indicate poor storage. They should be assessed before use because they can introduce contamination and hydrogen into the melt.
Q: How should magnesium ingots be stored?
Keep them dry and covered, away from acids, chlorides and heat sources. Magnesium reacts with moisture and is a fire hazard in finely divided form.
Q: Does the casting structure of an ingot matter?
Yes. A fine, uniform grain structure with low porosity and no inclusions gives consistent remelting behaviour and predictable recovery, which is particularly important for critical castings.