ZhenAn Alloy Cored Wire
1. The cored wire is flattened or broken and cannot be fed in.
Reasons: The core wire is empty, has less material, and is not tightly wrapped and leaks; the core wire is not round or solid; the steel strip is of poor quality; the rollers of the on-site wire feeding machine are too worn, which will cause the core wire to be pressed by the wire feeding machine If it is flat or the thread is broken, it cannot be fed. Solution: Adjust the equipment, cutting speed and calcium silicon alloy particle size to improve the quality of the cored wire, purchase qualified steel strips, and promptly report the wear of the rollers to the material unit.

Aluminum Calcium Wire
2. Bulk cored wire. Solution: Weld the core-wrapped coil firmly and add packing tape. Operating procedures for iron sheet slag retaining cones and clay slag retaining cones
1. From the iron slag-retaining cone, cut a sector-shaped piece with a radius of mm and a circumference of mm; from a clay slag-retaining cone, cut a sector-shaped piece with a radius of mm and a circumference of mm.
2. Hold it into a cone shape and solder the interface

CaFe Cored Wire
3. Add the prepared refractory clay into the cone and beat it firmly. The beaten refractory clay is 30mm away from the upper part of the iron sheet slag-stopping cone. Hold the 30mm iron sheet on the upper part of the iron sheet slag-stopping cone inward to prevent the strong refractory clay from falling off, and punch a 50mm-80mm deep round hole in the middle.
4. Store after drying