Sintering Temperature Control

The final sintering temperature of titanium carbide high-manganese-steel bonded cemented carbide is generally 1420 deg C. The sintering temperature should not be too high; the bonding phase may turn into a liquid phase and the metal may be lost, causing the hard phase to adjoin, aggregate, and grow, forming a source of fragmentation. The sintering temperature cannot be too low either, otherwise the alloy will be under-fired.

Vacuum Control

In addition to controlling the sintering temperature and speed, it is also necessary to control the degree of vacuum in the furnace during sintering, because too high a degree of vacuum will volatilize a large amount of liquid metal and cause component segregation. This is especially important in the three stages of degumming, reduction, and liquid phase sintering.

Heating Rate and Holding Time

The heating rate and holding time must be strictly controlled. In the low-temperature degumming stage, if the temperature rises quickly, the forming agent will not have time to volatilize, causing the compact to burst or micro-crack. In the reduction stage, the compact must be given enough time to remove volatile matter and oxygen from the raw material powder. When entering the liquid phase sintering stage, the temperature rise rate must also be slowed down to fully alloy the compact. The sintering principle of steel-bonded cemented carbide is the wetting principle, allowing the liquid phase to fully wet the solid phase.

Surface Decarburization Control

Industrial titanium plates with different compositions show different decarburization behaviors under the same conditions. For example, silicon can improve the elastic limit, strength, tempering stability, and elasticity loss resistance, but attention must also be paid to the severe surface decarburization caused by silicon increasing the activity of carbon in austenite. Low-carbon industrial titanium plate grades such as 28MnSiB reduce the carbon-silicon content, effectively reducing the tendency of surface decarburization while meeting the carbon content requirement.

Frequently Asked Questions

Why must the sintering temperature be controlled? Too high a temperature can cause metal loss and hard-phase aggregation, while too low a temperature leaves the alloy under-fired.

Why does vacuum degree matter during sintering? Excessive vacuum can volatilize liquid metal and cause component segregation.

How is surface decarburization reduced? By controlling composition, for example reducing the carbon-silicon content in low-carbon grades, and by managing the heating process.

Q: What is the final sintering temperature for titanium carbide high-manganese-steel bonded cemented carbide?
The final sintering temperature is generally 1420 deg C; it should not be too high or the bonding phase may turn into a liquid phase and metal may be lost.

Q: What happens if the sintering temperature is too high?
The bonding phase may become liquid and metal is lost, causing the hard phase to adjoin, aggregate, and grow, forming a source of fragmentation.

Q: Why must the vacuum degree be controlled during sintering?
Too high a degree of vacuum volatilizes a large amount of liquid metal and causes component segregation, especially in the degumming, reduction, and liquid phase sintering stages.

Q: Why must the heating rate be controlled in the low-temperature degumming stage?
If the temperature rises quickly, the forming agent has no time to volatilize, causing the compact to burst or micro-crack.

Q: How does silicon affect surface decarburization of titanium plates?
Silicon improves the elastic limit, strength, tempering stability, and elasticity loss resistance, but it increases the activity of carbon in austenite, so severe surface decarburization must be managed.