Mar 18, 2024 Leave a message

Abnormal phenomena in ferro titanium alloy smelting

1) When ferro titanium is smelted, the wet charge and the charge are mixed and boil, the furnace gas escapes unevenly, and the charge is sprayed out in large quantities.

2) The ferro ti charge is unevenly mixed and smelted unevenly.

 

Ferrotitanium

Titanium Ferro 30

 

3) The unit heat distribution is low, the reaction is slow, and the melting time of ferrotitanium is long. The reason is insufficient reducing agent, low calorific value or low charge preheating temperature, resulting in cold punching during melting.

4) The ferro titanium alloy smelting machinery unit has large heat distribution or high preheating temperature, violent reaction, stirring of slag, and slag spraying, which will lead to a reduction in ferrotitanium output.

 

Titanium Ferro

Titanium Ferro 40

Send Inquiry

Home