1. If the water content is too large, too much heat energy will be consumed when evaporating water, which will increase the power consumption of the submerged arc furnace. There is no national standard specifically for ferroalloy coke in China, and there are only corporate standards for some manufacturers. Most submerged arc furnaces that produce iron-containing gold still use metallurgical coke, screen coke and gasification coke.

Nitrided Ferro Chrome Lump
2. High fixed carbon content, low ash content, low content of harmful impurities such as Al2O3 and P2O5 in the ash, good coke reactivity, high coke resistivity, especially high temperature resistivity, low volatile matter, appropriate strength and suitability The lumpiness, less moisture and stability, etc. When the fixed carbon is high, the total amount of coke required is small, and the ash and harmful impurities brought in are relatively small. In this way, the amount of slag is small, the power consumption is low, and the alloy grade is high.

Medium Carbon Ferro Chrome Lump
3. Ferroalloy coke with large specific resistance can increase the resistance of the entire charge, increase the depth of electrode insertion, move the high temperature zone downward, expand the reaction zone, reduce the volatilization of reduced elements, improve heat utilization, and reduce power consumption. Ferroalloy coke should have appropriate strength, otherwise it will increase the amount of powdered coke, affect the air permeability of the furnace mouth surface, and lead to deterioration of furnace conditions. If the moisture content of ferroalloy coke fluctuates greatly, the amount of coke will not be easy to register, causing fluctuations in furnace conditions.