Physicochemical properties of ferromagnesia/ferroal spinel refractories
The chemical formula of Mgo-Fe2O3 is MgO·Fe2O3, of which MgO accounts for 20.16% and Fe2O3 accounts for 79.84%. It is a black mineral of equiaxed crystal system. n=1.78, hardness 7.8, relative density 4.1, coefficient of thermal expansion 7.1× 10-6k-1,1720℃ inconsistent melting into fe-containing liquid phase and cubic magnesite solid solution. These properties have important effects on the microstructure and physicochemical properties of magnesia iron bricks.

Only in the presence of metal Fe, can pure iron-aluminum spinel FeO·Al2O3 be produced. Therefore, it is best to use the electromelting process when synthesizing iron and aluminum spinel, or to add metal iron to burn under a strong reduction atmosphere. Under normal circumstances, the atmosphere in firing and use is neutral, and at best weak reducibility. Therefore, part of Fe2+ in ferro-aluminum spinel will be oxidized to Fe3+, and pure ferro-aluminum spinel will also be transformed into magnesia/magnesia/ferro-aluminum spinel or simply referred to as magnesia, ferro-aluminum composite spinel depending on the location.