Why Vacuum Treatment Is Used
High-carbon ferrochrome contains gases (mainly nitrogen and hydrogen) accounting for up to about 30 percent of the gas volume. When used in steelmaking, gas-bearing material can float on the interface between molten steel and slag, increasing the burning loss of chromium and reducing the recovery rate. Ferrochromium alloys containing bubbles also lose significant amounts of metal during crushing and packaging. The vacuum treatment of high carbon ferrochrome is a casting process adopted to reduce the alloy gas content.
The Treatment Process
The molten iron ladle filled with liquid ferrochrome is placed into the vacuum chamber. After sealing, a vacuum pump evacuates for about 5 to 7 minutes until the vacuum degree reaches 10.6 to 13.3 kPa. Then the vacuum is broken, the ladle is taken out, and casting proceeds.
Benefits
Vacuum treatment achieves the purpose of reducing inclusions and gases, making the surface of high-carbon ferrochrome smooth and flat, and reducing breakage and packaging losses. This improves the usable product yield and supports better chromium recovery during steelmaking.
Frequently Asked Questions
Why is vacuum treatment applied to high-carbon ferrochrome? To reduce the gas content (mainly nitrogen and hydrogen) and inclusions that reduce chromium recovery and cause metal loss.
What vacuum degree is used? About 10.6 to 13.3 kPa, with an evacuation time of about 5 to 7 minutes.
What are the benefits? Smoother surfaces, fewer inclusions and gases, and reduced breakage and packaging losses.