Jan 15, 2024 Leave a message

Causes Of Accidents Involving Material Collapse And Burns During High Carbon Ferrochromium Smelting

Lc Ferro Chrome Lump Price

 

1. The charge for high-carbon ferrochromium smelting is South African lump chromium ore, which has poor physical properties and is easy to dissolve and difficult to reduce. Coke has a high powder content and is accompanied by a certain amount of fine-grained blue carbon. It has low strength, poor electrical conductivity and air permeability, and is difficult to drop to the bottom of the furnace, causing a lack of carbon at the bottom of the furnace and causing excessive pressure in the furnace. During the smelting process, It is easy to cause material collapse and fire eruption.

 

Ferro Chrome

Hc Ferro Chrome Lump Price


The pole center circle of the electric furnace is too small, and the design of the electrode pole center circle is unreasonable during technical renovation. During smelting, the powder content of the material is too high, and the discharge is slow. The charge is reduced and melted quickly, and the material layer forms a fluffy material or cavity phenomenon. When adjusting the electrode feeding, it is easy to The furnace material surface collapses, causing splashing fire and scalding people.
      2. Violate safe operating procedures and fail to wear protective equipment correctly. During the production process, some smelting workers have weak safety awareness, paralysis of mind, and a sense of luck. They do not comply with safe operating procedures at their posts or are affected by habitual violations of regulations. During the operation, Failure to wear labor protection supplies (such as work clothes, protective masks, glasses, protective shoes, dust masks, etc.) as required and insufficient personal protection. When the furnace collapses and hot materials are ejected, the workers in front of the furnace are unable to dodge, increasing the number of human body injuries. Chance of getting burned.

 

High Carbon Ferro Chrome Low Silicon

Hc Ferro Chrome Lump


     3. The environmental condition of the production site is poor, the management of the work site is insufficient, the system and corrective measures are not implemented in place, and inspection and assessment are not strict, etc., resulting in the waste at the work site not being cleaned up in time, and the safe passages being narrow or occupied. When a danger of furnace collapse occurs, the safety passage (escape route) is blocked, making it impossible for workers to evacuate in time, which will increase the chance of an accident.
    4. Safety precautions are not implemented well. The operator on duty did not close the furnace door in time when the material was added to a certain level or after the material was completed. When encountering the danger of collapse of hot material in the furnace and ejection of hot material, due to working and resting near the furnace surface Improper positioning of personnel may lead to the risk of burns from hot material splashing from the furnace door.